Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.0 - 5.0 cP | 2.0 - 5.0 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 110 (5 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 2.0 - 5.0 cP | 2.0 - 5.0 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (5 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Viscosity | 2.0 - 5.0 cP | 2.0 - 5.0 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 110SI Surface Insensitive (20 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Viscosity | 2.0 - 3.0 cP @Temperature 25.0 °C |
2.0 - 3.0 cP @Temperature 77.0 °F |
Uncured |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Viscosity | 2.0 cP @Temperature 25.0 °C |
2.0 cP @Temperature 77.0 °F |
Uncured |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 2.0 cP @Temperature 25.0 °C |
2.0 cP @Temperature 77.0 °F |
Uncured |
Permabond 260 Cyanoacrylate PERMABOND 260 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 260 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates.. |
|||
Viscosity | 2.0 - 6.0 cP @Temperature 25.0 °C |
2.0 - 6.0 cP @Temperature 77.0 °F |
Uncured |
Permabond 919 Cyanoacrylate, High temperature Features & Benefits: Rapid development of high strength; Ease of use – no mixing or heat cure; Bonds most materials; 100% reactive, no solvents.PERMABOND® 919 is an allyl cyanoacrylate adhesive. I.. |
|||
Viscosity | 2.0 cP @Temperature 25.0 °C |
2.0 cP @Temperature 77.0 °F |
|
LyondellBasell PM Propylene glycol methyl ether Available in electronic grade.Information provided by Lyondell. |
|||
Viscosity | 2.0 - 20 cP | 2.0 - 20 cP | As Supplied |
Heraeus Cleviosâ„¢ P VP CH 8000 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP CH 8000 is an antistatic material based o.. |
|||
Viscosity | 2.0 - 3.0 cP | 2.0 - 3.0 cP | |
Solvay DURAPHOS® DBHP Dibutyl hydrogen phosphite Chemical Name: Dibutyl Hydrogen PhosphiteCAS: 1809-19-4Available in: Asia Pacific, Europe, Latin America and North AmericaChemical Formula: C8H19PO3Applications: DURAPHOS DBHP (Dibutyl Hydrogen Phos.. |
|||
Viscosity | 2.0 - 3.0 cP @Temperature 23.0 °C |
2.0 - 3.0 cP @Temperature 73.4 °F |
|
Master Bond MB300 Cyanoacrylate Adhesive System General purpose wicking grade, fills gap to 0.002Information provided by Master Bond Inc. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Loctite® 420 General Purpose Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Loctite® 493 General Purpose Methyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Loctite® 7649 Acetone Base Primer N Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Elmer's Products Aron Alpha® 101 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Superior tensile and shear strengths, well suited for metal bondingLow gap fill. Methyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substr.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Elmer's Products Aron Alpha® 201 Cyanoacrylate Adhesive (Industrial Krazy Glue™) General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Elmer's Products Aron Alpha® 221 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Elmer's Products Aron Alpha® 221F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Elmer's Products Aron Alpha® 401X Cyanoacrylate Adhesive (Industrial Krazy Glue™) Engineered for high temperature and high impact resistance.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. Ve.. |
|||
Viscosity | 2.0 - 5.0 cP | 2.0 - 5.0 cP | U-Tube IC-C45 |
3M Scotch-Weld™ MC5 Metal Instant Adhesive 3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC5 (formerly SP93) is a very low vi.. |
|||
Viscosity | 2.0 - 6.0 cP | 2.0 - 6.0 cP | ISO 3104/3105 |
3M Scotch-Weld™ MG05 PR Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Viscosity | 2.0 - 6.0 cP | 2.0 - 6.0 cP | ISO 3104/3105 |
3M Scotch-Weld™ PR5 Plastic and Rubber Instant Adhesive 3M™ Scotch-Weld™ Plastic and Rubber Instant Adhesive is designed to give exceptional performance on difficult-to-bond plastic and rubber substrates. This adhesive may be bonded to like substrates .. |
|||
Viscosity | 2.0 - 10 cP | 2.0 - 10 cP | |
3M Pronto™ CA-40 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.Very fast setting adhesive with.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
3M Scotch-Weld™ 3989 Anaerobic Adhesive Activators 3M™ Scotch-Weld™ Anaerobic Activators are general-purpose surface activators/primers that cure anaerobic adhesives or inactive or very cold surfaces. For normal active surfaces, 3M™ Scotch-Weld™.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
3M Scotch-Weld™ AC649 Anaerobic Adhesive Activators 3M™ Scotch-Weld™ Anaerobic Activators are general-purpose surface activators/primers that cure anaerobic adhesives or inactive or very cold surfaces. For normal active surfaces, 3M™ Scotch-Weld™.. |
|||
Viscosity | 2.0 - 5.0 cP | 2.0 - 5.0 cP | U-Tube IC-C45 |
3M Scotch-Weld™ SI5 Surface Insensitive Instant Adhesive 3M™ Scotch-Weld™ Surface Insensitive Adhesives bond rough, porous, contaminated, and acidic substrates including wood, cardboard, veneer, fabric, cork, and leather. SI5 (formerly SB20) is a very l.. |
|||
Viscosity | 2.0 - 4.0 cP | 2.0 - 4.0 cP | |
Oceanchem Group Tri-isobutyl Phosphate (TIBP) Molecular Formula: C12H27O4PCas No.: 126-71-6Chemical Properties: Ester property, it can be hydrolyzed in basic condition.Hazardous Features: It can be fired in heat, fire and oxidation condition, a.. |
|||
Viscosity | 2.0 - 4.0 cP @Temperature 25.0 °C |
2.0 - 4.0 cP @Temperature 77.0 °F |
Uncured |
Permabond 910FS Cyanoacrylate, Methyl grade PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts.. |
|||
Viscosity | 2.0 cP | 2.0 cP | |
Loctite® 7471 Acetone/Isopropanol Base Primer T Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |