Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 150 °C | 302 °F | |
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Middle Barrel Temperature | 150 °C | 302 °F | Blow Film |
DuPont Appeel® LSR11D554 Lidding Sealant Resin Appeel® LSR11D554 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals to poly.. |
|||
Middle Barrel Temperature | 150 °C | 302 °F | Blow Film |
DuPont Appeel® LSR20D745 Lidding Sealant Resin Appeel® LSR20D745 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu.. |
|||
Middle Barrel Temperature | 150 °C | 302 °F | Blow Film |
DuPont Appeel® LSR20D751 Lidding Sealant Resin Appeel® LSR20D751 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu.. |
|||
Middle Barrel Temperature | 150 °C | 302 °F | Blow Film |
DuPont Appeel® LSR11D625 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D625 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals .. |