Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 356 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 170 - 180 °C
338 - 356 °F
Multibase TPSiV® 4100-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
Middle Barrel Temperature 170 - 180 °C
338 - 356 °F
Multibase TPSiV® 4100-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Low compression setAPPLICATIONS: Solution for soft touch overmolding on consumer electr..
Middle Barrel Temperature 170 - 180 °C
338 - 356 °F
Multibase TPSiV® 4200-60A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Middle Barrel Temperature 170 - 180 °C
338 - 356 °F
Multibase TPSiV® 4200-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Middle Barrel Temperature 170 - 180 °C
338 - 356 °F
Multibase TPSiV® 4200-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane
Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem 8075 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem 8075 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem GP-785A TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem GP-785A TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem GP-915UB TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem GP-915UB TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem GP-930 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem GP-930 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem GP-950 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem GP-950 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem GP-975B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem GP-975B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem GP-980 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem GP-980 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem LP-870 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem LP-870 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem MP-845B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem MP-845B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem MP-930HD TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem MP-930HD TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Injection Molding
Stellarchem MP-855WR TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 160 - 180 °C
320 - 356 °F
Transition, Extrusion
Stellarchem MP-855WR TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Middle Barrel Temperature 150 - 180 °C
302 - 356 °F
Elastron® D SEBS Elastomer
Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureselectrical insulator with very low conductivityhas gra..
Copyright © lookpolymers.com All Rights Reserved