Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 140 - 249 °C | 284 - 480 °F | Average value: 198 °C Grade Count:130 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Die Temperature | 140 - 180 °C | 284 - 356 °F | |
Elastron® D SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureselectrical insulator with very low conductivityhas gra.. |
|||
Die Temperature | 140 - 170 °C | 284 - 338 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1582E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |