Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics, sound and vibration dampening, improved impact resistance, and U.V. stability. Elastocon® STK60 can be overmolded to polycarbonate, ABS, PC/ABS, Acrylic, HIPS, and various grades of nylon 6 and 6/6.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
ASTM D2240
Tensile Strength 5.37 MPa
779 psi
ASTM D412
Elongation at Break 568 %
568 %
ASTM D412
100% Modulus 0.00204 GPa
0.296 ksi
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 210 - 216 °C
410 - 420 °F
Front Barrel Temperature 216 - 266 °C
420 - 510 °F
Nozzle Temperature 227 - 277 °C
440 - 530 °F
Mold Temperature 26.7 - 48.9 °C
80.0 - 120 °F
Injection Velocity 25.4 - 127 mm/sec
1.00 - 5.00 in/sec
Back Pressure 0.517 - 1.21 MPa
75.0 - 175 psi