Processing Properties Metric English Comments
Back Pressure 0.517 - 1.21 MPa
75.0 - 175 psi
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™..
Back Pressure 0.517 - 0.862 MPa
75.0 - 125 psi
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding
PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec..
Back Pressure 0.517 - 1.21 MPa
75.0 - 175 psi
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer
Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s..
Back Pressure 0.517 - 1.21 MPa
75.0 - 175 psi
Elastocon TPE Technologies Elastocon® STK60B Thermoplastic Elastomer
Elastocon® STK60B black thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60B is well suited for ..
Back Pressure 0.517 - 1.21 MPa
75.0 - 175 psi
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer
Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer..
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA M-523
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA S310
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA S319
Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA S510
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA S610
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA S710
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA T-110
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA T-120
Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA TW-17
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA TW-18B2
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA TW-20
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA TW-23V
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA/PC TA-35
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 MPa
75.0 psi
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized
Data provided by Clariant Masterbatches
Back Pressure 0.517 - 1.21 MPa
75.0 - 175 psi
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer
Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s..
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Back Pressure 0.517 - 1.03 MPa
75.0 - 150 psi
Diamond Polymers ASA TWP 502
Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc.