Processing Properties Metric English Comments
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1001-177UV Thermoplastic Polyolefin, Non-UV Stabilized, HS5 Medium Dark Neutral
Applications: Scuff platesBodyside moldingsStep and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT1100-689UV Thermoplastic Polyolefin, UV Stabilized, Light Natural Beige
Applications: Pillar plugsAirbag doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold
Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products P251-00 Polypropylene Copolymer, Natural
Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products P256-00 Polypropylene Copolymer, Natural
Applications: Door/trunk scuffUnderhood componentsSplash shieldsElectrical enclosuresInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products P601-01 Polypropylene Copolymer, Black
Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black
Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 188 - 216 °C
370 - 420 °F
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 193 - 216 °C
380 - 420 °F
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed
black onlyInformation provided by MRC Polymers Inc.
Rear Barrel Temperature 177 - 216 °C
350 - 420 °F
Injection Molding
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
Rear Barrel Temperature 177 - 216 °C
350 - 420 °F
Injection Molding
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer
A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or..
Rear Barrel Temperature 177 - 216 °C
350 - 420 °F
Injection Molding
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer
A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj..
Rear Barrel Temperature 177 - 216 °C
350 - 420 °F
Injection Molding
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Rear Barrel Temperature 177 - 216 °C
350 - 420 °F
Injection Molding
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
Rear Barrel Temperature 199 - 216 °C
390 - 420 °F
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Rear Barrel Temperature 199 - 216 °C
390 - 420 °F
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Rear Barrel Temperature 182 - 216 °C
360 - 420 °F
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer
SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5..
Rear Barrel Temperature 182 - 216 °C
360 - 420 °F
CTC X-PRO CTC PP 2015 Polypropylene Impact Copolymer
X-PRO PP 2015 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Rear Barrel Temperature 182 - 216 °C
360 - 420 °F
CTC X-PRO PP 2050 Polypropylene Copolymer
X-PRO PP 2050 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Rear Barrel Temperature 204 - 216 °C
400 - 420 °F
CTC X-PRO TF 1140 HP Polypropylene Homopolymer, 40% Talc Filled
X-PRO TF 1140 HP is a 40% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, HVAC, and lawn ..
Rear Barrel Temperature 177 - 216 °C
350 - 420 °F
Injection Molding
Teknor Apex Sarlink® 4439D Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4439D is a high hardness grade possessing exceptional tensile strength, superior compression s..
Copyright © lookpolymers.com All Rights Reserved