Processing Properties Metric English Comments
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural
Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black
Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White
Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 210 - 238 °C
410 - 460 °F
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black
Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Rear Barrel Temperature 210 - 240 °C
410 - 464 °F
Start Point: 215°C
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
Start Point: 215°C
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
Start Point: 230°C
Kingfa MAC-301 PC/ABS Alloy
Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
Start Point: 230°C
Kingfa MAC-451 PC/ABS Alloy
Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
Gromax 1155LL TPE
1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex..
Rear Barrel Temperature 210 - 232 °C
410 - 450 °F
LTL Color Compounds ColorFast® ACR100 Polymethylmethacrylate
High heat injection molding grade of PMMAAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 210 - 232 °C
410 - 450 °F
LTL Color Compounds ColorFast® ACR100IM Polymethylmethacrylate, High Impact
High impact version, extrusion or injection molding PMMAAll information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 210 - 227 °C
410 - 440 °F
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled
For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc.
Rear Barrel Temperature 210 - 227 °C
410 - 440 °F
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled
For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc.
Rear Barrel Temperature 210 - 243 °C
410 - 469 °F
Styrolution NAS® 90 High Performance Styrenic
NAS® 90 has sparkling clarity, improved toughness, and good scratch resistance. This easily processed copolymer blends well with clear impact modifiers. It meets USP XXIII Spec. of Class VI Pla..
Rear Barrel Temperature 210 - 230 °C
410 - 446 °F
Unitika AX-1500 Conditioned
AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in..
Rear Barrel Temperature 210 °C
410 °F
Injection
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Rear Barrel Temperature 210 - 216 °C
410 - 421 °F
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer
Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume..
Rear Barrel Temperature 210 - 216 °C
410 - 420 °F
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer
Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer..
Rear Barrel Temperature 210 - 240 °C
410 - 464 °F
H-3
Denka STYROL MW1 Polystyrene
"DENKA SYTROL MW" is a well-balanced polystyrene (PS) resin, with a high tensile strength as well as good moldability. Overturning the traditional understanding that PS resin is "hard and brittle," ..
Rear Barrel Temperature 210 - 216 °C
410 - 421 °F
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer
Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer ..
Rear Barrel Temperature 210 - 220 °C
410 - 428 °F
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin
10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 210 °C
410 °F
Injection
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.