Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Nozzle Temperature = 530 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 260 - 277 °C
500 - 530 °F
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Nozzle Temperature 266 - 277 °C
510 - 530 °F
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate
Information provided by Ravago.
Nozzle Temperature 266 - 277 °C
510 - 530 °F
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate
Information provided by Ravago.
Nozzle Temperature 260 - 277 °C
500 - 530 °F
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Nozzle Temperature 249 - 277 °C
480 - 530 °F
LTL Color Compounds ColorFast® NY2115 Nylon 66
Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc.
Nozzle Temperature 254 - 277 °C
490 - 530 °F
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Nozzle Temperature 254 - 277 °C
490 - 530 °F
Wellman Wellamid® GS40-60 42L-N 40% Glass Sphere Filled Nylon 6, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Nozzle Temperature 227 - 277 °C
440 - 530 °F
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer
Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s..
Nozzle Temperature 227 - 277 °C
440 - 530 °F
Elastocon TPE Technologies Elastocon® STK60B Thermoplastic Elastomer
Elastocon® STK60B black thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60B is well suited for ..
Nozzle Temperature 227 - 277 °C
440 - 530 °F
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer
Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer..
Nozzle Temperature 266 - 277 °C
510 - 530 °F
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
Nozzle Temperature 266 - 277 °C
510 - 530 °F
Entec Hylex® P1317FR Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Nozzle Temperature 227 - 277 °C
440 - 530 °F
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer
Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s..
Copyright © lookpolymers.com All Rights Reserved