Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 1080ZG90 Metal Filled Polyamide

Category Polymer , Thermoplastic , Nylon
Manufacturer Ecomass Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 1080ZG90 Metal Filled Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityMetal Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 5.50 g/cc
5.50 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm
0.0050 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.4 MPa
6000 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Tensile Modulus 6.45 GPa
935 ksi
ASTM D638
Flexural Strength 51.7 MPa
7500 psi
ASTM D790
Flexural Modulus 6.65 GPa
965 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 204 - 254 °C
400 - 490 °F
Mold Temperature 57.2 - 82.2 °C
135 - 180 °F
Drying Temperature 73.9 °C
165 °F
Dry Time 4 hour
4 hour
Users viewing this material also viewed the following: