Huntsman Araldite EPN 9880 CH Epoxy Phenol Novolac

Category Polymer , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name Araldite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Araldite EPN 9880 CH Epoxy Phenol Novolac.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Weight per Epoxide (EEW, g/eq) 171 to 185. Max color is 5.Comments/Applications: Unmodified, low viscosity phenol novolac with a functionality of 3.6. High performance (chemical and heat resistance) coatings and tank linings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 18000 - 25000 cP
18000 - 25000 cP