Electrical Properties Metric English Comments
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1050TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Techn..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1080TU95 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1080TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1080ZD92 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade
High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1080ZD95 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1080ZD96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1080ZG90 Metal Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityMetal Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by T..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding
High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1700CO94 Copper Powder Filled Polyamide, Injection Molding
High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform..
Surface Resistivity per Square 0.21 ohm
0.21 ohm
ASTM D257
Ecomass® 1700TU96 Tungsten Filled Polyamide
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyRigidInformation provided by Technical Po..