Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Eastar GN071 Natural PETG Copolyester

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , PETG Copolyester
Manufacturer Eastman Chemical
Trade Name Eastar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Eastar GN071 Natural PETG Copolyester.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions will not turn EASTAR GN071 white.Applications: MedicalPreliminary Data Sheet Comments: Properties reported here are based on limited testing. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.Information provided by Eastman Chemical.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 0.13 %
0.13 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.0035 cm/cm

@Thickness 3.20 mm
0.0035 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Ultimate 27.0 MPa
3920 psi
ISO 527
30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 49.0 MPa
7110 psi
ASTM D638 and ISO 527
Elongation at Break 110 %
110 %
ISO 527
Elongation at Yield 4.0 %
4.0 %
ISO 527
Tensile Modulus 2.02 GPa
293 ksi
ISO 527
Flexural Yield Strength 69.0 MPa
10000 psi
ISO 178
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched 0.980 J/cm
1.84 ft-lb/in
ASTM D256
0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ISO 75
Optical Properties Metric English Comments
Haze 0.30 %
0.30 %
ASTM D1003
Transmission, Visible 91 %
91 %
Total Transmittance; ASTM D 1003
Processing Properties Metric English Comments
Melt Temperature 260 °C
500 °F
Mold Temperature 27.0 °C
80.6 °F
Drying Temperature 71.0 °C
160 °F
Dry Time 5 hour
5 hour
Users viewing this material also viewed the following: