Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.980 J/cm @Temperature -30.0 °C |
1.84 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature -30.0 °C |
1.84 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARPEEK 50 G/30 30% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature -30.0 °C |
1.84 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors. |
|||
Izod Impact, Notched | 0.980 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-702 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
Kolon Kopa® KN173HI Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333C22 CF Reinforced Nylon 66 Carbon 22%, high strengthApplications Cylinder piston partsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
Lotte Chemical Titan TITANZEX® HB6200 High density polyethylene HB6200 is a high density polyethylene for blow molding. HB6200 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. Applic.. |
|||
Izod Impact, Notched | 0.980 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-722 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE003Z PC LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 553M PBT+PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | Light & White Colors; ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | Light & White Colors; ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL INT1512 PPE+HIPS (Asia Pacific) PPE/HIPS GF filled for auto interior |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
Toyobo PELPRENE™ S9002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Izod Impact, Notched | 0.980 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NYLON 6001GF33 33% Glass Filled Polyamide Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
Eastman Eastar GN071 Natural PETG Copolyester EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions wi.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® G702H Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® G703H Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® G703V Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 90G33 33% Glass Filled Nylon 66 Enhanced strength and stiffness; with 33% GF. Superior fluidity and appearance.Applications:Automotive parts Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM 3.2mm |