Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | >= 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 0.980 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-722 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE003Z PC LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade. |
|||
Izod Impact, Notched | 0.980 J/cm @Temperature 23.0 °C |
1.84 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 553M PBT+PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | Light & White Colors; ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | Light & White Colors; ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® EM-8250G MPPE, 20% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1102 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-1801 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9100SG ASA, Unreinforced Used for solid vinyl door, frame etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® FD-1102 PC, FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trihip® B500 High Impact Polystyrene Dimensional stability, electrical properties and weather resistance are excellent.B500 is the non-flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, P.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trimma® SD6350H PMMA, Opaque High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm |
1.84 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® DMH3000S Polycarbonate, High Flow Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.DMH3000S is a high flow, flame retardant grade.Applications: LCD TV Front cover, high .. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® P305G20 PP, 20% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL INT1512 PPE+HIPS (Asia Pacific) PPE/HIPS GF filled for auto interior |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® P305G30 PP, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T883GV25 Flame Retardant PBT, 25% Glass Fiber |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH50G2 20% Glass Fiber Reinforced High Strength Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 90G33 33% Glass Filled Nylon 66 Enhanced strength and stiffness; with 33% GF. Superior fluidity and appearance.Applications:Automotive parts Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.980 J/cm | 1.84 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® G702V Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 0.981 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.84 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G5 Nylon 66, 25% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Izod Impact, Notched | 0.981 J/cm | 1.84 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® JN100 PPE+PA66 Filler Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |