Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
Elongation at Break >= 50 %
>= 50 %
Nominal
Elongation at Yield 30 %
30 %
Tensile Modulus 1.40 GPa
203 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 600 V
600 V