Eastman 1830A Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman 1830A Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyethylene 1830A meets the requirements of FDA regulations at 21 CFR 177.1520 (c) (2.2) and may be used as a component of packages used for holding food during cooking.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D 4883
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.7 MPa
1700 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 10.7 MPa
1550 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 500 %
500 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.207 GPa
30.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection