Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2209 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2242 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2405 20% Ethylene-Methyl Acrylate Copolymer
(discontinued **) Westlake EMAC® SP2405 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperature are required. SP2405 provides.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman D4027-P Voridian Polyethylene
(discontinued **) VORIDIAN low density polyethylene D4027-P is a formulation suggested for extrusion coating applications that require clarity, high gloss and superior hot tack properties. Applications/UsesFood Packa.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | ASTM D746 |
Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding
(discontinued **) Product Description: TENITE Polyethylene 1810A contains NO ADDITIVES. It is suggested for injection molding applications. TENITE Polyethylene 1810A meets the requirements of FDA regulation 21 CFR 1.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 1550A Polyethylene
(discontinued **) Injection molding gradeUnless otherwise noted, all tests are run at 23°C and 50% RH. Where required, samples are compression molded per ASTM D1928.Information from manufacturer data sheet.Eastman .. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 1810A Polyethylene
(discontinued **) Polyethylene 1810A contains no additives. It is suggested for injection molding applications.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to West.. |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | ASTM D746 |
Eastman 1810E Polyethylene
(discontinued **) Polyethylene 1810E contains no additives. It is suggested for general purpose extrusion applications requiring good stress crack resistance or electrical properties. It is used in applications suc.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 1830E Polyethylene
(discontinued **) Polyethylene 1830E is a low density formulation. It is suggested for general purpose extrusion applications, such as tubing and blow molding. Polyethylene 1830E meet the requirements of FDA regula.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 808A Polyethylene
(discontinued **) Low density polyethylene 808A is a general-purpose formulation used for injection molding and general-purpose extrusion.Unless otherwise noted, all tests are run at 23°C and 50% RH.Information from.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman 808E Polyethylene
(discontinued **) Low density polyethylene 808E is a general-purpose formulation used general-purpose extrusion. Under regulations administered by the US FDA, 808E may lawfully be used as articles or components of a.. |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | ASTM D746 |
Eastman E6838-862A Polyethylene
(discontinued **) E6838-862A is a low density formulation suggested for injection molding applications, such as closuresInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemic.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Eastman M2004-P Polyethylene
(discontinued **) M2004-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M2004-P has been found to exhibit good barrier properties, temperature res.. |
|||
Brittleness Temperature | -73.0 - -65.0 °C | -99.4 - -85.0 °F | Average value: -70.3 °C Grade Count:3 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EBAC® SP1802 22.5% Ethylene Butyl Acrylate Copolymer Westlake EBAC® SP1802 is a 22.5% EBA copolymer designed for blown film, tie-layer, coextrusions and blending where flexibility and strength are important. SP1802 provides excellent elasticity and l.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EBAC® SP1806 17.5%, Ethylene-Methyl Acrylate Copolymer Description: Westlake EBAC® SP1806 is an ethylene butyl acrylate copolymer designed for extrusion coating and laminating. SP1806 can also be compounded as an impact modifier or used in highly fill.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® Plus SP1305 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1305 is a 20% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1305 is.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® Plus SP1307 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1307 is a 20% EMA copolymer designed for extrusion coating, laminations, and blending where EMA properties are needed, but higher temperature resistance is required. SP1307 is.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2207 20% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2207 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficient of friction.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2260 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2260 is a 24% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2260 provide.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2268 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2268 is a 24% EMA copolymer designed for extrusion coating, tie-layers, compounding, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM-D746 |
Westlake EMAC® SP2404 18.5% EMA Copolymer Westlake EMAC� SP2404 is a 18.5% EMA copolymer designed for blown film, tie-layer, coextrusions, and blending where flexibility and strength are important. SP2404 provides excellent elasticity .. |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM-D746 |
Westlake EMAC® SP2409 20% EMA Copolymer Westlake EMAC� SP2409 is a 20% EMA copolymer designed for extrusion coating, tie-layers, and extrusions where flexibility, compatibility, low heat seal temperatures, or a high coefficient of fr.. |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | |
Dow Corning SILASTIC® LCS-740 SILICONE RUBBER 40 Durometer, translucent, low compression set, uncatalysed Silicone Rubber Base suitable for molding.Information provided by Dow Corning |
|||
Brittleness Temperature | -73.0 °C | -99.4 °F | |
Dow Corning SILASTIC® LCS-755 SILICONE RUBBER 55 Durometer, translucent, low compression set, uncatalysed Silicone Rubber Base suitable for molding.Information provided by Dow Corning |
|||
Brittleness Temperature | <= -73.0 °C | <= -99.4 °F | ASTM D746 |
Westlake EMAC® SP2403 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2403 is a 24% EMA copolymer designed for extrusion coating, tie-layers, compounding, and extrusions where flexibility, compatibility, low heat seal temperatures, or high coefficien.. |
|||
Brittleness Temperature | -73.0 - -60.0 °C | -99.4 - -76.0 °F | Average value: -69.8 °C Grade Count:4 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu.. |