Tensile Strength, Ultimate 11.7 - 13.8 MPa
1700 - 2000 psi
ASTM D638-95
Multibase Multi-Flex® TPO 1047 (AH)
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.
Tensile Strength, Ultimate 11.7 - 15.1 MPa
1700 - 2190 psi
ASTM D638-95
Multibase Multi-Flex® TPO DEFA 1047
The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase.
Tensile Strength, Ultimate 11.7 MPa
1700 psi
TM R050-36
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
TM R050-36
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman 1830A Polyethylene  (discontinued **)
Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyet..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman 1830E Polyethylene  (discontinued **)
Polyethylene 1830E is a low density formulation. It is suggested for general purpose extrusion applications, such as tubing and blow molding. Polyethylene 1830E meet the requirements of FDA regula..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman E6838-862A Polyethylene  (discontinued **)
E6838-862A is a low density formulation suggested for injection molding applications, such as closuresInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemic..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
ASTM D638
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Base resin for fully formulated low voltage cable i..
Tensile Strength, Ultimate 11.7 - 44.0 MPa
1700 - 6380 psi
Average value: 30.1 MPa Grade Count:80
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
ASTM D638
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Sylvin Technologies 8980-75 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Sylvin Technologies 9077-95 LMW Natural PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Sylvin Technologies 9980-75 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Sylvin Technologies 9999-95 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Heat aged 2 weeks at 175°C
DuPont Vamac® DP Sartomer 350 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Cecilia 20 aged 168 hrs at 175°C
DuPont Vamac® DP Activator OC Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
508 mm/min; ASTM D638
Dow Engage® ENR 7256.00 Ethylene-Butene Copolymer
Description: ENR 7256.00 is a unique broader molecular weight distribution ethylene-butene copolymer with higher branching levels that offers excellent clarity, processing and performance in foams a..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
ASTM D638
Colorite Polymers 6077 Non-Phthalate 77 Series Vinyl Compound
Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Colorite Polymers 6511 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Colorite Polymers 6512 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Colorite Polymers Self Frosting™ 6511SF Vinyl Compound
Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
ASTM D412; ISO 37; DIN 53504
Advanced Polymer Alloys Alcryn® 2165 NC Melt Processable Rubber
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
ASTM D638
Colorite Polymers 6575 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 11.7 - 20.7 MPa
1700 - 3000 psi
Average value: 16.1 MPa Grade Count:7
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min..
Tensile Strength, Ultimate 11.7 - 27.1 MPa
1700 - 3930 psi
Average value: 19.5 MPa Grade Count:10
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer  (discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
Tensile Strength, Ultimate 11.7 MPa
1700 psi
Bond strength to metal
Dymax Light Weld® 429 High Clarity Glass Bonding Adhesive
Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond..