Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 1550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D412
Polymax® Maxelast® P3785 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 10.7 MPa
1550 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman 1830A Polyethylene  (discontinued **)
Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyet..
Tensile Strength, Yield 10.7 MPa
1550 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Eastman 1830E Polyethylene  (discontinued **)
Polyethylene 1830E is a low density formulation. It is suggested for general purpose extrusion applications, such as tubing and blow molding. Polyethylene 1830E meet the requirements of FDA regula..
Tensile Strength, Yield 10.7 MPa
1550 psi
Molded; ASTM D638
LyondellBasell Petrothene® NA963083 Low Density Polyethylene
ApplicationsPETROTHENE NA 963 is a series of resins formulated with special antiblock additive and designed for a wide variety of industrial film applications where high impact strength and excellen..
Tensile Strength, Yield 10.7 MPa
1550 psi
@50% Elongation; ASTM D1414
Greene Tweed FLUORAZ® 790 Fluoroelastomer, FEPM
Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f..
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D412
Teknor Apex APEX® 3300-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me..
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D412
Teknor Apex APEX® 90-A41R-60-NT Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D412
Teknor Apex APEX® 3200-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Tensile Strength, Yield 10.7 MPa
1550 psi
Dow LDPE 510I Low Density Polyethylene
DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It..
Tensile Strength, Yield 10.7 MPa
1550 psi
Dow Primacor® 4608 Ethylene Acrylic Acid (EAA)
PRIMACOR® 4608 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating resin. It is designed to provide excellent adhesion to metallic, paper and polyethylene substrat..
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Axiall 59996J Moldings & Extrusions Flexible PVC
Injection and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Axiall 8610 Moldings & Extrusions Flexible PVC
A high quality, low gravity, clear extrusion and molding compound with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Bapolene® 2292 Polyethylene Film Grade
Bapolene 2292 is a butene linear low density polyethylene copolymer designed to provide a combination of toughness and stiffness and complies with FDA 21 CFR177.1520.Applications: Closures, lids, an..
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Axiall 50896 Moldings & Extrusions Flexible PVC
Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 10.7 MPa
1550 psi
ASTM D-638
Axiall 8603 Moldings & Extrusions Flexible PVC
A soft extrusion compound with rubber-like properties and oil resistance. Ideally suited for extruded profiles, tubings and co-extruded shapes.Information provided by Georgia GulfGeorgia Gulf becam..