Material Notes:
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C510 which predominates in North America, alloy C519 is generally used in Europe.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Annealed
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 703 - 807 MPa
102000 - 117000 psi
Tensile Strength, Yield 689 - 793 MPa
100000 - 115000 psi
0.2% offset
Elongation at Break >= 1.0 %
>= 1.0 %
in 2 in.
Tensile Modulus 117 GPa
17000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 60.5 W/m-K
420 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 93.9 %
93.9 %
Phosphorous, P 0.10 %
0.10 %
Tin, Sn 6.0 %
6.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000119 ohm-cm
0.0000119 ohm-cm
Annealed
Users viewing this material also viewed the following: