Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.81 g/cc | 0.318 lb/in³ | |
Indium Corp. Indalloy 53 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Special Metals MONEL® Alloy R-405 The free-machining version of MONEL alloy 400. A controlled amount of sulfur is added to the alloy to provide sulfide inclusions that act as chip breakers during machining. Other characteristics a.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Goodfellow Havar® High Permeability Nickel Magnetic Alloy A high Nickel, magnetically soft alloy used for magnetic shielding, high quality low noise audio frequency transformers, ground fault interrupter cores, anti-shoplifting devices, tape recorder head .. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 220 Commercial Bronze, 1/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 220 Commercial Bronze, 3/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 220 Commercial Bronze, Extra Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 519 Phosphor Bronzes 6%, 1/2 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 519 Phosphor Bronzes 6%, Extra Spring Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 519 Phosphor Bronzes 6%, Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Annealed Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | Annealed |
Eagle Brass 521 Phosphor Bronzes 8% C, Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1 H13 3/4 hard, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1 H14 4/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1C 0 Annealed, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TB Wire quenched Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TDX Rod quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TH2 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX DECLAFOR® 1015 THX Wire quenched/Precipitation Heat Treated Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1 H11 1/4 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1 H15 Spring, Drawn Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
CLAL-MSX ARCAP Anticorrosion AP1D H14 4/4 hard, Drawn Copper Alloy, Wire and rod, diameter High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In par.. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Cadi 10 MOLD-MOR™ A Copper Nickel Silicon Chromium Alloy with high thermal conductivity and moderate hardness.Information provided by Cadi Company. |
|||
Density | 8.80 g/cc | 0.318 lb/in³ | |
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or .. |