Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 110 EPT COPPER, 1/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 110 EPT COPPER, 3/4 Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 110 EPT COPPER, Annealed Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 151 ZHC® COPPER, 1/2 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 151 ZHC® COPPER, Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 151 ZHC® COPPER, Spring Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 18665 MSP1, 1/2 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 18665 MSP1, 1/4 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 19210 XP-10 Copper Iron, 1/2 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 19210 XP-10 Copper Iron, 3/4 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 19210 XP-10 Copper Iron, Extra Spring 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 19210 XP-10 Copper Iron, Spring 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 210 Gilding Metal, Annealed CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 210 Gilding Metal, Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 220 Commercial Bronze, 1/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 220 Commercial Bronze, 3/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 220 Commercial Bronze, Annealed CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 220 Commercial Bronze, Extra Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 220 Commercial Bronze, Extra Spring CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 230 Red Brass, 3/4 Hard CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 230 Red Brass, Extra Spring CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 519 Phosphor Bronzes 6%, 1/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 519 Phosphor Bronzes 6%, 3/4 Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 519 Phosphor Bronzes 6%, Extra Hard Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 519 Phosphor Bronzes 6%, Extra Spring Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 101 OFE COPPER (Certified), Annealed Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 101 OFE COPPER (Certified), Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 102 OF COPPER (Non-Certified), 1/2 Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 102 OF COPPER (Non-Certified), Extra Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Modulus | 117 GPa | 17000 ksi | |
Eagle Brass 102 OF COPPER (Non-Certified), Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |