Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 703 - 807 MPa
102000 - 117000 psi
Eagle Brass 519 Phosphor Bronzes 6%, Extra Spring
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..