Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 689 MPa | >= 100000 psi | |
Niagara LaSalle StressProof® Cold Finished Steel Bar StressProof® is made by a patented process which consists of drawing the bar through a special die under heavy draft, then stress relieving it in a precisely controlled furnace. StressProof® offer.. |
|||
Tensile Strength, Yield | 689 MPa | 100000 psi | |
Pacific Sintered Materials FN-253-S(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-100HTAll information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 689 - 869 MPa | 99900 - 126000 psi | 0.2% proof |
Kobe Steel KS15-3-3-3 Beta Titanium Alloy, AMS 4914, Solution treated Nominal Composition: Ti-15 V-3 Cr-3 Sn-3 AlApplications: Aircraft parts, bicycle gears, gold club heads, foils. Features:Cold workable.Information provided by Kobe Steel |
|||
Tensile Strength, Yield | 689 MPa @Strain 0.200 % |
100000 psi @Strain 0.200 % |
|
Materion moldMAX® XL Spinodally Hardened Copper-Nickel-Tin Alloy moldMAX XL® is a unique spinodally hardened copper-nickel-tin alloy that combines high strength and high thermal conductivity. Available in large plate thickness up to 12†and in rounds up t.. |
|||
Tensile Strength, Yield | 689 MPa | 99900 psi | 3 inches; Un-Nitrided |
Latrobe LSSâ„¢ 135M Nitriding Steel (ASTM A355 Class A) TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured fr.. |
|||
Tensile Strength, Yield | 689 MPa | 100000 psi | Hard |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Tensile Strength, Yield | >= 689 MPa @Strain 0.200 % |
>= 100000 psi @Strain 0.200 % |
|
Universal Wire Works 901 (AMS 5660) Nickel Alloy Filler Metal Alloy 901 is a corrosion and heat resistant nickel-base alloy designed for gas tungsten arc and gas metal arc welding. Alloy 901 is used primarily for parts, such as turbine rotors, shafts and bucke.. |
|||
Tensile Strength, Yield | 689 - 1240 MPa | 100000 - 180000 psi | depending on condition of material after heat treatment |
Universal Wire Works 17-4 (AMS 5825) Filler Metal Universal 630 (17Cr-4Ni) is a martensitic precipitation - age hardening stainless steel alloy. Alloy 630 can be welded with all welding processes without preheat; however, to obtain weld metal prope.. |
|||
Tensile Strength, Yield | >= 689 MPa | >= 100000 psi | 0.2% Offset |
Eagle Brass 430 Ferritic Stainless Steel, Full Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Tensile Strength, Yield | 689 - 793 MPa | 100000 - 115000 psi | 0.2% offset |
Eagle Brass 519 Phosphor Bronzes 6%, Extra Spring Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C.. |
|||
Tensile Strength, Yield | 689 - 779 MPa | 100000 - 113000 psi | 0.2% offset |
Eagle Brass 521 Phosphor Bronzes 8% C, Spring Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Yield | >= 689 MPa | >= 100000 psi | 0.2% offset |
Eagle Brass 70265 XP175, Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 689 MPa | 99900 psi | Strip (TH04) |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Tensile Strength, Yield | 689 MPa @Strain 0.200 % |
100000 psi @Strain 0.200 % |
Solution treated ~ 34 HRC |
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli.. |
|||
Tensile Strength, Yield | 689 MPa | 100000 psi | Hard |
California Fine Wire Alloy 52 Nickel Iron Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 689 MPa | 100000 psi | Hard |
California Fine Wire Dumet Nickel Iron Core Copper Clad Alloy All values may vary dependent on specific design and usage99.9% copper cladding over iron-nickel coreCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength, Yield | 689 - 827 MPa @Strain 0.200 % |
99900 - 120000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TM04 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 689 MPa | 99900 psi | |
Ametek High Purity Nickel Strip 899E 50% Cold-Rolled Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 689 MPa @Temperature 22.0 °C |
100000 psi @Temperature 71.6 °F |
Heat Treated to 24-32 HRC |
Schmolz + Bickenbach Holder Block Plastic Mold Steel Description: Holder Block is a modified AISI-4130 material with higher chromium and molybdenum content specifically designed holder steel for molds and dies and The material is forged on a 5000 ton.. |