A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced, Impact Modified
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 69
69
ASTM D785
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Flexural Modulus 2.89 GPa
419 ksi
ASTM D790
Izod Impact, Notched 2.65 J/cm
4.96 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C
243 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D648