EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Carbon Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties: high stiffness and strengthvery low densityexcellent notched impact resistance also at low temperatureslow creephigh heat distortion temperaturesvery low moisture absorptionvery good dimensional stability and little warpageexcellent UV-resistanceelectrically conductivelow wear and coefficient of friction The product has been designed for injection molding of technical parts especially in the area of die-cast metal replacement of highest performance. Grilamid LCL-3H anthracite is used in the following market segments: sports and leisure articlesmechanical engineeringhousehold and appliances The carbon-fibers are aligned in parallel and are just as long as the pellets (usually 10 mm).Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 1.1 %
1.1 %
ISO 62
Moisture Absorption 0.600 %
0.600 %
ISO 62
Linear Mold Shrinkage, Transverse 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 135 MPa
19600 psi
conditioned; ISO 2039-1
Tensile Strength at Break 250 MPa
36300 psi
conditioned; ISO 527-1/-2
Elongation at Break 1.7 %
1.7 %
conditioned; ISO 527-1/-2
Tensile Modulus 19.0 GPa
2760 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
conditioned; ISO 179/1eU
Charpy Impact, Notched 2.80 J/cm²
13.3 ft-lb/in²
conditioned; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 160 °C
320 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
conditioned; IEC 60093
Surface Resistance 50 ohm
50 ohm
IEC 60093
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Cooling and climate control
Exterior
Fuel systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Long Fiber Reinforced
Special Characteristics Anti-static
Improved heat resistance