ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer ATI Allvac
Trade Name Vasco®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Vasco® 9310 Specialty Steel, Heat Treatment: 899°C (1650°F) Normalization.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: High performance helicopter transmission gears, components.
Physical Properties Metric English Comments
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 334
334
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 363
363
Estimated from Rockwell C value.
Hardness, Rockwell C 36
36
Hardness, Vickers 349
349
Estimated from Rockwell C value.
Tensile Strength, Ultimate 966 MPa
140000 psi
Tensile Strength, Yield 897 MPa

@Strain 0.200 %
130000 psi

@Strain 0.200 %
Elongation at Break 15 %
15 %
Reduction of Area 40 %
40 %
Component Elements Properties Metric English Comments
Carbon, C 0.11 %
0.11 %
Chromium, Cr 1.2 %
1.2 %
Iron, Fe 94 %
94 %
as balance
Manganese, Mn 0.55 %
0.55 %
Molybdenum, Mo 0.12 %
0.12 %
Nickel, Ni 3.3 %
3.3 %
Phosphorous, P 0.013 %
0.013 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.013 %
0.013 %