Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ELASTO UK Mediprene™ 500600M TPE, Medical Applications, 60A Hardness

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Mediprene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Mediprene™ 500600M TPE, Medical Applications, 60A Hardness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low extractableNo migration of plasticizerCleanlinessGood vapor and gas transmission propertiesSoftness, flexibility and clarityChemical inertnessEase of sterilization for repeated useMediprene™ compounds can be processed using conventional thermoplastic equipment for extrusion, injection molding, etc. The compounds are not hygroscopic, and thus do not need any pre-drying. Assembling Mediprene™ to mainly all used thermoplastics is feasible.All Mediprene™ grades are fully recyclable and where possible reprocessable during manufacturing and when burned do not emit toxic fumes.Mediprene™ grades exhibit excellent resistance to many fluids used in the healthcare environment.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Melt Flow 1.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Thickness 4.00 mm
60

@Thickness 0.157 in
ASTM D2240
Tensile Strength at Break 12.0 MPa
1740 psi
ASTM D638
Elongation at Break 700 %
700 %
ASTM D638
100% Modulus 0.00170 GPa
0.247 ksi
ASTM D638
300% Modulus 0.00280 GPa
0.406 ksi
ASTM D638
Tear Strength 29.0 kN/m
165 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Processing Properties Metric English Comments
Processing Temperature 180 - 210 °C
356 - 410 °F
Descriptive Properties Value Comments
Chemical Resistance Good
Excluding organic solvents, aromatic and vegetable oils
Color Translucent
Weather Resistance Good