Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00170 GPa | 0.247 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Vistaflex® 671N Thermoplastic Rubber
(discontinued **) A translucent thermoplastic elastomer with snappiness. It can be processed using injection molding or extrusion processing techniques.Key Features: Flex modulus (1% Secant) 9.0 MPa (1300 psi); Vica.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | TPE-0153 (ASTM D 412) |
ExxonMobil Vyram™ 9271-55 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use, as well as rubber articles in contact with non-fatty, non-oily foods as closure.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4445 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4445 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | ISO 37 |
ELASTO UK Dryflex® 5014-101 TPE, Modified Injection Molding Grade for General Applications The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 5014-101 is specifically designe.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | ISO 37 |
ELASTO UK Dryflex® 8013-101 Flame Retardant TPE for Extrusion, Black Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | ISO 37 |
ELASTO UK Dryflex® 8013-101 Flame Retardant TPE for Injection Molding, Black Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | ASTM D638 |
ELASTO UK Mediprene™ 500600M TPE, Medical Applications, 60A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Molded Golf Grips FormulationNordel® IP 4640 |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5656 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 281-55 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | ISO 37 |
AlphaGary Evoprene™ 075 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00170 GPa | 0.247 ksi | ISO 37 |
AlphaGary Evoprene™ 076 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |