E-Polymers TEKAMID® TB120G45 , 45% Glass Fiber Reinforced PA6, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAMID® TB120G45 , 45% Glass Fiber Reinforced PA6, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
45% Glass Fiber Reinforced, High Strength.Information provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
23°C/24 hr; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ASTM D786
Tensile Strength, Yield 200 MPa
29000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 280 MPa
40600 psi
ASTM D790
Flexural Modulus 11.5 GPa
1670 ksi
ASTM D790
Izod Impact, Notched 1.80 J/cm
3.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D2133
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 90.0 - 110 °C
194 - 230 °F