Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® HTR8351 NC021 Polyester Elastomer TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer DuPont Performance Polymers
Trade Name Hytrel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR8351 NC021 Polyester Elastomer TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30 Shore D Easy-to-Strip UV Stabilized Polyester Elastomer with Non-discoloring Stabilizer Developed for Extrusion Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4 2577
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 190 °C
10 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 21
21
15s; ISO 868
Tensile Strength at Break 9.00 MPa
1310 psi
ISO 527-1/-2
Tensile Stress 1.10 MPa

@Strain 5.00 %
160 psi

@Strain 5.00 %
ISO 527-1/-2
2.10 MPa

@Strain 10.0 %
305 psi

@Strain 10.0 %
ISO 527-1/-2
5.30 MPa

@Strain 50.0 %
769 psi

@Strain 50.0 %
ISO 527-1/-2
Elongation at Break 210 %
210 %
ISO 527-1/-2
Tensile Modulus 0.0170 GPa
2.47 ksi
ISO 527-1/-2
Tear Strength 54.0 kN/m
308 pli
normal; ISO 34-1
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Part Marking Code >TPC-ET<
ISO 11469
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification TPC-ET
ISO 1043
Special Characteristics Light stabilised or stable to light
U.V. stabilised or stable to weather
Users viewing this material also viewed the following: