Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 308 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 54.0 kN/m
308 pli
ASTM D624
Multibase Multi-Flex® TPE A 9305 BLK
This product was developed for one shot airbag covers with improved stiffness and low temperature resistance. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 54.0 kN/m
308 pli
73°F, Die C; ASTM D624
ExxonMobil Santoprene® 283-40MED Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..
Tear Strength 54.0 kN/m
308 pli
Trouser Tear Resistance, MD; ISO 6383-1
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Tear Strength 53.9 kN/m
308 pli
50mm/min, @ Break; ASTM D624
LG Chemical KEYFLEX TO1192A Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7, 1333-86-4 and 9002-88-4Information provided by LG Chemical
Tear Strength 54.0 kN/m
308 pli
Die B, no post cure; ASTM D624
Multibase C6-570 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 54.0 kN/m
308 pli
ASTM D624
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
Tear Strength 54.0 kN/m
308 pli
ASTM D2240
UBE UBEPOL VCR412 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C)
Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel..
Tear Strength 54.0 kN/m
308 pli
DIN 53515
Lubrizol ESTANE® 58866 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 54.0 kN/m
308 pli
GB/T 529
Chengdu Polyster 8500 General Grade TPV
Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 54.0 kN/m
308 pli
73°F, Die C; ASTM D624
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Tear Strength 54.0 kN/m
308 pli
73°F, Die C; ASTM D624
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Tear Strength 54.0 kN/m
308 pli
normal; ISO 34-1
DuPont Performance Polymers Hytrel® HTR8351 NC021 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D Easy-to-Strip UV Stabilized Polyester Elastomer with Non-discoloring Stabilizer Developed for Extrusion Information provided by DuPont Performance Polymers
Tear Strength 54.0 kN/m
308 pli
Parallel to flow; ISO 34-B
AlphaGary Evoprene™ GF 6257 Automotive Thermoplastic Elastomer
Evoprene™ GF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
Tear Strength 54.0 kN/m
308 pli
Trouser Tear Resistance, MD; ISO 6383-1
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Copyright © lookpolymers.com All Rights Reserved