Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.10 MPa @Strain 100 % |
305 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3660T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.10 MPa @Strain 300 % |
305 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3838 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.10 MPa @Strain 200 % |
305 psi @Strain 200 % |
ASTM D412 |
Teknor Apex Monprene® MP-2815A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 2.10 MPa @Strain 300 % |
305 psi @Strain 300 % |
ASTM D412 |
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Tensile Stress | 2.10 MPa @Strain 300 % |
305 psi @Strain 300 % |
ASTM D412 |
ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced us.. |
|||
Tensile Stress | 2.10 MPa @Strain 0.160 %, Temperature 180 °C |
305 psi @Strain 0.160 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per.. |
|||
Tensile Stress | 2.10 MPa @Strain 10.0 % |
305 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® EL250 TPC-ET Injection Molding |
|||
Tensile Stress | 2.10 MPa @Strain 10.0 % |
305 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8351 NC021 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D Easy-to-Strip UV Stabilized Polyester Elastomer with Non-discoloring Stabilizer Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.10 MPa @Strain 5.00 % |
305 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients.. |
|||
Tensile Stress | 2.10 MPa @Strain 5.00 % |
305 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.10 MPa @Strain 300 % |
305 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P55A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P55A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.10 MPa @Strain 300 % |
305 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P55A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P55A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |