Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by A.D. Compound
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Filler Content 40 %
40 %
ISO 3451 / 1
Melt Index of Compound 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
ISO 868
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Elongation at Yield 5.0 %
5.0 %
ISO 527
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
Izod Impact, Notched (ISO) 2.90 kJ/m²
1.38 ft-lb/in²
ISO 180/1A
Izod Impact, Unnotched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75
Vicat Softening Point 97.0 °C
207 °F
49 N; ISO 306