Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1.10 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.10 MPa

@Strain 100 %
160 psi

@Strain 100 %
Across Flow; ISO 37
PolyOne OnFlex™ HT 50A-3S2099 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
Tensile Stress 1.10 MPa

@Strain 100 %
160 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 1.10 MPa

@Strain 100 %
160 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S HF 50A-3S1981 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 1.10 MPa

@Strain 100 %,
Temperature 21.0 °C
160 psi

@Strain 100 %,
Temperature 69.8 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ HC 9210-45N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-45N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgic..
Tensile Stress 1.10 MPa

@Strain 100 %
160 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P1740 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.10 MPa

@Strain 10.0 %
160 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 1.10 MPa

@Strain 3.28 %,
Temperature 100 °C
160 psi

@Strain 3.28 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..
Tensile Stress 1.10 MPa

@Strain 5.00 %
160 psi

@Strain 5.00 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR8351 NC021 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D Easy-to-Strip UV Stabilized Polyester Elastomer with Non-discoloring Stabilizer Developed for Extrusion Information provided by DuPont Performance Polymers