Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection molding and extrusion.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.233 g/cc
0.04454 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0129 cm/cm
0.0129 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore D 61

@Temperature 23.0 °C,
Time 15.0 sec
61

@Temperature 73.4 °F,
Time 0.00417 hour
ISO 868
67

@Temperature 23.0 °C,
Time 1.00 sec
67

@Temperature 73.4 °F,
Time 0.000278 hour
ISO 868
Tensile Strength at Break 34.0 MPa

@Temperature 23.0 °C
4930 psi

@Temperature 73.4 °F
ISO 527
Tensile Strength, Yield 20.0 MPa

@Temperature 23.0 °C
2900 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 330 %

@Temperature 23.0 °C
330 %

@Temperature 73.4 °F
nominal; ISO 527
350 %

@Temperature 23.0 °C
350 %

@Temperature 73.4 °F
ISO 527
Elongation at Yield 29 %

@Temperature 23.0 °C
29 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 0.290 GPa

@Temperature 23.0 °C
42.1 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 1.30 J/cm²

@Temperature -30.0 °C
6.19 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 211 °C
412 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ISO 75-1/-2
Processing Properties Metric English Comments
Melt Temperature 245 °C
473 °F
Optimum; Extrusion
245 °C
473 °F
Optimum; Injection Molding
240 - 250 °C
464 - 482 °F
Extrusion
240 - 250 °C
464 - 482 °F
Injection Molding
Mold Temperature 45.0 °C
113 °F
optimum; Injection Molding
Drying Temperature 80.0 - 100 °C
176 - 212 °F
Extrusion
80.0 - 100 °C
176 - 212 °F
Injection Molding
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Injection Molding
2.00 - 4.00 hour
2.00 - 4.00 hour
Extrusion
Moisture Content <= 0.050 %
<= 0.050 %
Extrusion
<= 0.10 %
<= 0.10 %
Injection Molding
Descriptive Properties Value Comments
Appearance Natural Color
Forms Pellets
Generic TPC-ET
Material Status Current
Part Marking Code >TPC-ET<
ISO 11469
Processing Method Injection Molding, Extrusion
Product Category Extrusion Resins
Region Available - Global Yes
Resin Identification TPC-ET
ISO 1043
RoHS Compliance Contact Manufacturer
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved