Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.233 g/cc | 0.04454 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET
(Unverified Data**) Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like .. |