Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | 75/Method Bf |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | |
Reliance Industries Polypropylene - Wollastonite filled Information provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CR120CL Polypropylene, Random Copolymer, Clarified, Lubricated Random clarified copolymer specially formulated to achieve high clarity and excellent color and color stability with excellent mold release properties. Applications: Injection molding applications s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 678C Polystyrene
(discontinued **) STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer Key Features: excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive parts, luggage, totes, bins, carrying cases, appliancesMeets FDA requirement.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Flint Hills P5M6K-080 Polypropylene Random Copolymer Features: Clarified, Gamma Radiation Sterilizable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: Disposable Syringes. This product is not rec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | ASTM D648 |
Ineos T50-500-171 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ISO 75-1, -2 |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ISO 75B |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacomâ„¢ 6551 Polypropylene Homopolymer Description: Hostacomâ„¢ 6551 conventional melt flow, 1,300 MPa flexural modulus, precolored polypropylene homopolymer has a good combination of strength, stiffness, impact and heat resistance. I.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific) LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ISO 75-2 |
Borealis Daplen™ VB4411 TPO Compound Daplen VB4411 is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen VB4411 is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Annealed; ISO 75-2A |
Total PSC 1810/1811 Polystyrene 1811 is a very easy flowing crystal polystyrene designed, principally, for the injection molding industry. The excellent processing characteristics of this grade allows for the production of articl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Entec Hypro™ PP-CP4/2 Impact Copolymer, 4 Melt Flow This is intended for use in injection molding applications for automotive and consumer products and also contains a long term heat aging additive package.Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Diamond Polymers SBS 1001 Styrene Butadiene Block Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | Unannealed; ASTM D648 |
Dow DS6D21 Polypropylene Random Copolymer Resin OverviewConsistent processabilityHigh clarity and glossComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D21 Polypropylene Resin is intended for use in case film processes. It is particularly su.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.1 °C | 178 °F | unannealed; molded and tested in accordance with ASTM D 4101; ASTM D648 |
Dow DS6D21 Polypropylene Resin DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Busine.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | |
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 - 101 °C | 178 - 214 °F | Average value: 94.2 °C Grade Count:19 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Stat-kon MD000IU PP (Asia Pacific) LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data wa.. |