Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | 75/Method Bf |
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | |
Reliance Industries Polypropylene - Wollastonite filled Information provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CR120CL Polypropylene, Random Copolymer, Clarified, Lubricated Random clarified copolymer specially formulated to achieve high clarity and excellent color and color stability with excellent mold release properties. Applications: Injection molding applications s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET
(Unverified Data**) Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Flint Hills AP7710-HS Impact Copolymer Polypropylene TPO copolymer, UL certified, and FDA compliant.Features: Structural stiffness, ultra high impact strength, and high uniform flow rate.Applications: Injection molding: automotive items and exterior e.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Flint Hills P5M6K-080 Polypropylene Random Copolymer Features: Clarified, Gamma Radiation Sterilizable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: Disposable Syringes. This product is not rec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648-97 |
Ipiranga Petrochem PCC 0710 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648-97 |
Ipiranga Petrochem PRB 4215 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ISO 75-1, -2 |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ISO 75B |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
LyondellBasell Astryn SD068-4 Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, high modulus, mineral-filled, blow molding and extrusion grade polypropylene copolymer, good melt strength, excellent processability, excellent impact and stiffne.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS LNP* STAT-LOY A3000T is a compound based on ABS. Added features of this grade include: Antistatic, Clear. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Asia Pacific) LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific) LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | Annealed; ISO 75-2A |
Total PSC 1810/1811 Polystyrene 1811 is a very easy flowing crystal polystyrene designed, principally, for the injection molding industry. The excellent processing characteristics of this grade allows for the production of articl.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Entec Hypro™ PP-CP4/2 Impact Copolymer, 4 Melt Flow This is intended for use in injection molding applications for automotive and consumer products and also contains a long term heat aging additive package.Information provided by Entec |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM D648 |
Diamond Polymers SBS 1001 Styrene Butadiene Block Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | ASTM-D648 |
Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer PCD 0810 is a high melt flow rate heterophasic copolymer developed for injection molding applications. The product combines high impact strength and good processability with a fair stiffness level. .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C | 178 °F | |
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 - 101 °C | 178 - 214 °F | Average value: 94.2 °C Grade Count:19 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |