Polymer Property : Linear Mold Shrinkage, Transverse = 0.0124 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
Plastcom SLOVALEN PQ 81 T 10 PP, 10% mineral filling
FeaturesModified PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene..
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
STN 64 0808
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a..
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre
FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
Linear Mold Shrinkage, Transverse 0.0124 cm/cm

@Thickness 2.00 mm
0.0124 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® SK645FR BK851 PBT  (Unverified Data**)
Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P..
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
ISO 294-4
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET  (Unverified Data**)
Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like ..
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
60x60x2 mm; ISO 294
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT
Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so..
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
Plastcom SLOVALEN PQ 83 T 10 PP, 10% mineral filling
FeaturesModified PP + EPDM for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal. Decreased shrinkage. Application in automotive, covers of car chas..
Linear Mold Shrinkage, Transverse 0.0124 cm/cm
0.0124 in/in
Plastcom SLOVASTER® B1 GF 30 PBT, 30% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..