Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced, Impact Grade
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. Processing methods include injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
cm³/10min; ISO 1133
2.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
Nominal; ISO 527-1/-2
Elongation at Yield 33 %
33 %
ISO 527-1/-2
Tensile Modulus 1.30 GPa
189 ksi
ISO 527-1/-2
Flexural Strength 35.0 MPa

@Strain 3.50 %
5080 psi

@Strain 3.50 %
ISO 178
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eA
1.70 J/cm²

@Temperature -30.0 °C
8.09 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 111 °C
232 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Emissions <2 mg/kg
VDA 275
Part Marking Code >POM-HI<
ISO 11469
Processing Blow Moulding
Coatable
Injection Moulding
Other Extrusion
Profile Extrusion
Sheet Extrusion
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM-HI
ISO 1043