Thermal Properties Metric English Comments
Melting Point 88.0 °C
190 °F
Internal Method
Polimeri Europa Greenflex® MH 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Extrusion
Greenflex MH 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and extrusion. Items produced with Greenflex MH 40 show high elasticity and good mechanical properties.Main Applic..
Melting Point 88.0 °C
190 °F
Internal Method
Polimeri Europa Greenflex® FD 50 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 50 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FD 50 exhibit good optical and sealing properties, high flexibility and toughnes..
Melting Point 88.0 °C
190 °F
Internal Method
Polimeri Europa Greenflex® FD 53 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FD 53 is an ethylene vinyl acetate copolymer (EVA), containing antiblocking agent, for blown film extrusion. Films produced with Greenflex FD 53 exhibit good sealing properties, high flex..
Melting Point 88.0 °C
190 °F
Exxon Method
ExxonMobil Escorene® LD-708 EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal ..
Melting Point 88.0 °C
190 °F
DTA
DuPont™ Surlyn® 9970 Ionomer Resin, Zinc  (discontinued **)
Surlyn® 9970 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Melting Point 88.0 °C
190 °F
DSC; ASTM D3418
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Melting Point 88.0 - 91.0 °C
190 - 196 °F
M Chemical GUARD DOGâ„¢ UV1164 Light Absorber, Triazene Derivative
GUARD DOGâ„¢ UV1164 light stabilizer is a derivative of Triazine that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout t..
Melting Point 88.0 - 128 °C
190 - 262 °F
Hybrid Plastics POSS® MA0717 MethacrylEthyl-POSS®
POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®..
Melting Point 88.0 °C
190 °F
Freezing Point via DSC/ASTM D3418
DuPont Elvax® 3165SB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Melting Point 88.0 °C
190 °F
TRN-14
Tipco Tipcolite® TPG 1214 - Furfural Modified Phenolic Resin with 43mm Norton Flow with 9% Hexamine
Furfural Modified Phenolic Resin with 43mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: High Heat AbrasivesInformation provided by the Manufacturer, Tipco Industries L..
Melting Point 88.0 °C
190 °F
Freezing point via DSC/ASTM D3418
DuPont Bynel® 3930 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 87.8 °C
190 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 713.93 Cast Film Resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin..
Melting Point 87.8 °C
190 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile..
Melting Point 87.8 °C
190 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil EXACT™ 4151 Plastomer for Cast Film
Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer multilayer coextru..
Melting Point 88.0 °C
190 °F
ASTM D3418, ISO 3146
DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate
Elvaloy® AC 12024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®..
Melting Point 88.0 °C
190 °F
DSC
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium
Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Melting Point 88.0 °C
190 °F
DSC
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions ..
Melting Point 88.0 °C
190 °F
DSC
DuPont™ Surlyn® PC350 Ionomer Resin, Highest Clarity, Sodium
Surlyn® PC350 luxury molding resin is a "select" grade of Surlyn® 8945, controlled to achieve the highest possible optical clarity in molded perfume jars and caps, while being optimized for proces..
Melting Point 88.0 °C
190 °F
ASTM D3418, ISO 3146
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate
Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®..
Melting Point 88.0 - 90.0 °C
190 - 194 °F
BASF Imidazole
Formula: C3H4N2CAS: 288-32-4Description: Imidazole is a crystalline powder with an amine-like odor. It is soluble in water.Synonyms: 1,3-Diaza-2,4-cyclopentadiene, 1,3-Diazole, Imidazol, Methanimid..
Melting Point 88.0 °C
190 °F
Aquabond Technologies Aquabond™ ABS-85 Water Soluble Adhesive and Bonding Thermoplastic
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem..
Melting Point 88.0 °C
190 °F
10°C/min
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema.
Melting Point 88.0 °C
190 °F
10°C/min
Arkema Group Evatane® 1020 VG 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high mechanical properties. Examples: films, chemical bags, gloves.ISO data provided by the manufactur..
Melting Point 88.0 °C
190 °F
ASTM D3417
DuPont Elvax® 3165Z Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 3165Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives..
Melting Point 88.0 °C
190 °F
ASTM D3417
DuPont Elvax® 3172Z Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 3172Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additives..
Melting Point 88.0 °C
190 °F
DSC
Arkema Group LOTRYL® 16 MA 003 Copolymer Ethylene - Methyl Acrylate
LOTRYL® 16 MA 003 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the methyl acrylate content, LOTRYL® 16 MA 003 is a polymer o..
Copyright © lookpolymers.com All Rights Reserved