Material Notes:
VORANOL™ 4701C polyether polyol is a high reactivity capped triol. Its nominal 4800 molecular weight and primary hydroxyl content make it well suited for the production of high resiliency, flexible molded foams.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.019 g/cc
1.019 g/cc
Viscosity Measure 61 cSt

@Temperature 98.9 °C
61 cSt

@Temperature 210 °F
435 cSt

@Temperature 37.8 °C
435 cSt

@Temperature 100 °F
860 cSt

@Temperature 25.0 °C
860 cSt

@Temperature 77.0 °F
4500 cSt

@Temperature 0.000 °C
4500 cSt

@Temperature 32.0 °F
Maximum Moisture Content 0.050
0.050
wt% water
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
ASTM Color <= 50
<= 50
APHA
Thermal Properties Metric English Comments
Specific Heat Capacity 2.08 J/g-°C

@Temperature 20.0 °C
0.497 BTU/lb-°F

@Temperature 68.0 °F
2.27 J/g-°C

@Temperature 60.0 °C
0.543 BTU/lb-°F

@Temperature 140 °F
2.46 J/g-°C

@Temperature 100 °C
0.588 BTU/lb-°F

@Temperature 212 °F
Thermal Conductivity 0.151 W/m-K
1.04 BTU-in/hr-ft²-°F
0.123 W/m-K

@Temperature 100 °C
0.852 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.126 W/m-K

@Temperature 40.0 °C
0.875 BTU-in/hr-ft²-°F

@Temperature 104 °F
Flash Point 185 °C
365 °F
Optical Properties Metric English Comments
Refractive Index 1.4542
1.4542
Chemical Properties Metric English Comments
Total Acid Number 0.030
0.030
[mg/g]
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 32 - 36