Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.08 J/g-°C @Temperature 20.0 °C |
0.497 BTU/lb-°F @Temperature 68.0 °F |
|
Dow VORANOL™ 4701 Polyether Polyol VORANOL™ 4701 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.Informa.. |
|||
Specific Heat Capacity | 2.08 J/g-°C @Temperature 20.0 °C |
0.497 BTU/lb-°F @Temperature 68.0 °F |
|
Dow VORANOL™ 4701C Polyether Polyol VORANOL™ 4701C polyether polyol is a high reactivity capped triol. Its nominal 4800 molecular weight and primary hydroxyl content make it well suited for the production of high resiliency, flexibl.. |