Material Notes:
Description: Highly substantive to hair and skin. Recommended for high conditioning shampoos and moisturizing body washes. Enhances deposition of actives such as silicone, anti-dandruff agents and moisturizing oils.Chemical Name: Guar Gum DerivativeC.T.F.A./I.N.C.I. Name: Guar Hydroxypropyltrimonium ChlorideCAS: 65497-29-2Solubility: Soluble in water at 20°C. Insoluble in non-plar solventAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: JAGUAR C-17 is a highly charged cationic plant derived polymer. It provides excellent thickening and conditioning properties for hair and skin care products and improves active deposition onto hair. Ideal for use in conditioning shampoos, cream rinses, bath and shower products, lotions, creams and other personal care products. Recommended use levels: 0.1 – 0.3% Note: Viscosity develops immediately after JAGUAR C-17 has been dispersed into water under stirring and adjusted to a slightly acidic pH (pH = 3.5 – 5.0) with citric acid for example.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
Particle Size >= 90 µm
>= 90 µm
thru 150 Mesh; RP-0887
pH 8.5 - 10.5
8.5 - 10.5
Inherent 1%; RP-0889
Viscosity 2000 - 4000 cP

@Time 7200 sec
2000 - 4000 cP

@Time 2.00 hour
RP-0942
Component Elements Properties Metric English Comments
Nitrogen, N 1.5 - 2.1 %
1.5 - 2.1 %
Extracted; RP-0885
Processing Properties Metric English Comments
Moisture Content 5.0 - 9.5 %
5.0 - 9.5 %
RP-0838
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Creamy white fine powder
RP-0884
Composition Gram Negative Bacteria
Negative, RP-1445
Molds and yeasts
<100 cfu/g, RP-1445
Plate Count
<300 cfu/g, RP-1410
Staphylococcus Aureus
Negative, RP-1445
Odor Slight, characteristic (Pass)
RP-0359
Users viewing this material also viewed the following: