Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vapor Pressure = 0.0000133 bar Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Vapor Pressure 0.0000133 bar

@Temperature 20.0 °C
0.0100 torr

@Temperature 68.0 °F
LyondellBasell Glycol Ether DBA Diethylene glycol butyl ether acetate
Information provided by Lyondell.
Vapor Pressure <= 0.0000133 bar

@Temperature 20.0 °C
<= 0.0100 torr

@Temperature 68.0 °F
LyondellBasell TPNB Tripropylene glycol normal butyl ether
Information provided by Lyondell.
Vapor Pressure <= 0.0000133 bar

@Temperature 20.0 °C
<= 0.0100 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Solvesso™ 200 ND Aromatic Fluid
Appearance: Transparent - Slight Yellow LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Dow SPECFLEX™ NC 630 Polyol
SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082..
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Dow SPECFLEX™ NC 700 Polyol
SPECFLEX™ NC 700 polyol is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile. It is manufactured without the use of BHT and has been filtered to 200 microns. CA..
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Dow VORALUX™ HL 430 Copolymer Polyol
VORALUX™ HL 430 is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile and filtered to 100 microns. It is used in the manufacture of flexible slabstock polyurethan..
Vapor Pressure 0.0000133 bar
0.0100 torr
Dow VORANATE™ T-80 toluene diisocyanate (TDI)
VORANATE™ T-80 TDI products are designed for a variety of high-resilience molding, TDI molding, formulating (systems) and flexible slabstock applications. They are used in the production of flexib..
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Dow VORANOL™ 4240 Polyether Polyol
VORANOL™ 4240 polyether polyol is a nominal 4000 molecular weight diol based on propylene oxide with ethylene oxide capping. Its high molecular weight and enhanced reactivity make it well suited t..
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Dow VORANOL™ 4701C Polyether Polyol
VORANOL™ 4701C polyether polyol is a high reactivity capped triol. Its nominal 4800 molecular weight and primary hydroxyl content make it well suited for the production of high resiliency, flexibl..
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Dow VORANOL™ 4703 Polyether Polyol
VORANOL™ 4703 polyether polyol is a nominal 5000 molecular weight, high reactivity capped triol. It has a high primary hydroxyl content making it suitable for use in making all types of high resil..
Vapor Pressure 0.0000133 bar

@Temperature 25.0 °C
0.00998 torr

@Temperature 77.0 °F
BASF Lupranate® T80 Toluene Diisocyanate
Description: Lupranate® T80 toluene diisocyanate (TDI) is an 80% - 20% mixture of the 2,4 and 2,6 isomers of toluene diisocyanate. This product is used in the preparation of polyurethane foams, pre..
Vapor Pressure 0.0000133 bar

@Temperature 25.0 °C
0.00998 torr

@Temperature 77.0 °F
BASF Lupranate® TF2115 Isocyanate
Description: Lupranate® TF2115 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric-MDI) enriched with monomeric-MDI.Information provided by BASF
Vapor Pressure 0.0000133 bar

@Temperature 25.0 °C
0.00998 torr

@Temperature 77.0 °F
BASF Lupranate® 8020 Isocyanate
Description: Lupranate® 8020 Isocyanate is an 80:20 weight percent combination of toluene diisocyanate (TDI) and polymethylene polyphenylisocyanate (polymeric MDI). This product is used in the prep..
Copyright © lookpolymers.com All Rights Reserved