Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.126 W/m-K @Temperature 40.0 °C |
0.875 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
Dow VORANOL™ 4701 Polyether Polyol VORANOL™ 4701 polyether polyol is a high reactivity capped triol. Its high molecular weight and high primary hydroxyl content make it well suited for high resiliency, flexible molded foams.Informa.. |
|||
Thermal Conductivity | 0.126 W/m-K @Temperature 40.0 °C |
0.875 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
Dow VORANOL™ 4701C Polyether Polyol VORANOL™ 4701C polyether polyol is a high reactivity capped triol. Its nominal 4800 molecular weight and primary hydroxyl content make it well suited for the production of high resiliency, flexibl.. |