A. Schulman POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ Light Grey LL803366/4 Concentrate Based In LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® LL80366/4 is a light grey color concentrate based in LLDPE. This concentrate was designed to provide opacity and color in blow molding applications. POLYBATCH® LL80366/4 is heavy metal free and is typically recommended for use at 4% addition levels. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Melt Flow 51 g/10 min

@Load 2.16 kg,
Temperature 190 °C
51 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Ash 51 %
51 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789