C.O.I.M. FILCO® 306 Film Former for Glass Fiber Sizes

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name FILCO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. FILCO® 306 Film Former for Glass Fiber Sizes.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Typical Physical and Chemical Characteristics: Filco 306 is an epoxy resin in non-ionic water emulsionpure epoxy resinepoxy equivalent ~ 330narrow particle size distributionhydrolysis and sedimentation stability from pH 2 to 12 min. 48 hgood shelf lifehigh mechanical shear stability of the diluted emulsionCharacteristics of the dried film: cleartacky filmfilm less soft then the film for Filco 309compatible with unsaturated polyester, epoxy, phenolic matricesquickly soluble in styreneApplications: Filco 306 is suggested as a film former for glass fiber sizes for: filament winding rovingpultrusion rovingwoven rovingInformation provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Solids Content 48 - 52 %
48 - 52 %
MA145LFE
Particle Size 0.15 - 0.60 µm
0.15 - 0.60 µm
MA147LFE
pH 5.5 - 7.5
5.5 - 7.5
MA148LFE
Viscosity 1000 - 2000 cP

@Temperature 25.0 °C
1000 - 2000 cP

@Temperature 77.0 °F
spindle n 3-10 RPM; MA143LFE
Descriptive Properties Value Comments
Appearance Milky Liquid
Epoxy Equivalent on Dry Resin 300-360
(g), MA149LFE